Contact us For product pricing, customization, or other inquiries:
Contact Us
Explore More Products
- Product Details
- {{item.text}}
Quick Details
-
CaO Content (%):
-
0.1%
-
CrO Content (%):
-
0.01
-
SiC Content (%):
-
88
-
Place of Origin:
-
Henan, China
-
Model Number:
-
RON
-
Brand Name:
-
Lite
-
Product name:
-
Reaction sintered silicon carbide beam/batts as kiln furniture
-
raw material:
-
Silicon carbide powder
-
Color:
-
black
-
Feature:
-
Good thermal shock resistance
-
Density:
-
2.8g/cm3
-
apparent porosity:
-
12%
-
max working temperature:
-
1450℃
-
Usage:
-
kiln car of Ceramic kiln
-
Certificate:
-
test report
Quick Details
-
SiO2 Content (%):
-
5%
-
Al2O3 Content (%):
-
1%
-
MgO Content (%):
-
0.02%
-
CaO Content (%):
-
0.1%
-
CrO Content (%):
-
0.01
-
SiC Content (%):
-
88
-
Place of Origin:
-
Henan, China
-
Model Number:
-
RON
-
Brand Name:
-
Lite
-
Product name:
-
Reaction sintered silicon carbide beam/batts as kiln furniture
-
raw material:
-
Silicon carbide powder
-
Color:
-
black
-
Feature:
-
Good thermal shock resistance
-
Density:
-
2.8g/cm3
-
apparent porosity:
-
12%
-
max working temperature:
-
1450℃
-
Usage:
-
kiln car of Ceramic kiln
-
Certificate:
-
test report
Oxidation firing nitride bonded Silicon carbide plate/ ceramic kiln shelf/SiC batt
| Properites | Units | Silicon carbide Material | ||||
| Type | SiC | SiSiC | NSiC | RSiC | ||
| SiC% | 89 | 87 | 92 | 70 | 99 | |
| SiO2 % | 5 | 6 | - | Si3N4 28 | - | |
| Al2O3% | 1 | 2 | - | - | - | |
| Bulk Desity | g/cm3 | 2.85 | 2.8 | 3.01 | 2.8 | 2.75 |
| Apparent porosity | % | 12 | 14 | 0.1 | 12 | 14 |
| M.O.R.@20℃ | MPa | 50 | 48 | 260 | 180 | 100 |
| M.O.R.@1300℃ | MPa | 58 | 56 | 280 | 185 | 120 |
| C.T.E.@20℃-1000℃ | 10-6K-1 | 4.8 | 4.2 | 4.5 | 4.7 | 4.6 |
| C.C.S | MPa | 100 | 90 | 900 | 500 | 300 |
| ℃ | 1450 | 1420 | 1300 | 1500 | 1650 | |